Sample Preparation Procedure Metadata

Lakefield Research, Lakefield, Ontario / Grain Mount: 0.25 – 0.50 mm



Procedure Description

Laboratory: Lakefield Research, Lakefield, Ontario

Method: Grain Mount: 0.25 – 0.50 mm

The mineral grains were polished and mounted in epoxy on 25 mm diameter lucite disks (standard electron microprobe mounts).

Sample Classification (Preparation)

IndexSample CountSurveySample BundleSample TypePrep Lab MaterialDuplicates count
210001210298 Till Grain Mount: 0.25 – 0.50 mm
210001210980 Till Grain Mount: 0.25 – 0.50 mm
613  210001210981 Till Grain Mount: 0.25 – 0.50 mm611 
116  210006210293 Till Grain Mount: 0.25 – 0.50 mm115 
501  210006210954 Till Grain Mount: 0.25 – 0.50 mm501 
1656  210006210955 Till Grain Mount: 0.25 – 0.50 mm1651 
352  210006210955 Esker Grain Mount: 0.25 – 0.50 mm352 
452  210007210301 Till Grain Mount: 0.25 – 0.50 mm449 
47  210012210306 Till Grain Mount: 0.25 – 0.50 mm45 
10  138  210013210312 Till Grain Mount: 0.25 – 0.50 mm138 
11  132  210041210318 Till Grain Mount: 0.25 – 0.50 mm131 
12  69  210042210322 Till Grain Mount: 0.25 – 0.50 mm65 
13  527  210247210009 Heavy Mineral Concentrate Grain Mount: 0.25 – 0.50 mm521 
14  999  210248210009 Heavy Mineral Concentrate Grain Mount: 0.25 – 0.50 mm976 
Date modified: